Add to Favorites
Share

Pink Aluminum Oxide

  • Description
Product Detail


    Instruction:

    Pink fused alumina looks pink, because is electrically fused in high temperature, being added with the right quantity of oxidized chromium. Its hardness is close to, but toughness higher than that of WA.

    It's an abrasive material with moderate friability, recommended for tool and internal grinding, grinding jobs in instrument industry. It's also suitable for various grinding purpose with high surface finish.


    Chemical composition:

    Grit

    Low chromium

    Medium chromiumHigh chromium

    Al2O3
    (%) 

     Cr2O3
    (%) 

    Na2O
    (%)

    Al2O3
    (%)

    Cr2O3
    (%)

    Na2O
    (%) 

    Al2O3
    (%)

    Cr2O3
    (%)

    Na2O
    (%) 

    F12-F80

    =98.50

    0.20-0.45

    =0.50

    =98.20

    >0.45-1.00

    =0.55

    =97.40

    >1.00-2.00

    =0.55

    F90-F150

    =98.50

    =0.50

    =98.20

    =0.60

    =97.00=0.60

    F180-F220

    =98.50

    =0.50

    =98.80

    =0.70

    =96.50=0.70


    Physical property:

    Basic minerals

    Crystal size
    µm 

    True density
    g/cm3

    Bulk density
    g/ cm3

    Knoop hardness
    kg/mm2

    a-Al2O3

    600-2000

    =3.90

    1.40-1.91

    2200-2300

Send your message to this supplier
To:  

Dragon Abrasives Group Limited

* Content:  

For better quotations, include:

- A self introduction

- Special requests, if any

Quantity:  

  
Not exactly what you want? One request, multiple quotations Get Quotations Now >>